Show simple item record

dc.creatorMoliński, Waldemar
dc.creatorRoszyk, Edward
dc.creatorJabłoński, Aleksander
dc.creatorPuszyński, Jakub
dc.creatorCegieła, Janusz
dc.date2016-10-01
dc.date.accessioned2023-03-13T20:58:29Z
dc.date.available2023-03-13T20:58:29Z
dc.identifierhttps://revistas.ubiobio.cl/index.php/MCT/article/view/2555
dc.identifier.urihttps://revistaschilenas.uchile.cl/handle/2250/224016
dc.descriptionMechanical parameters of ash wood (Fraxinus excelsior) subjected to compression in radial direction, before and after its thermal modification and measured at moisture content close to the equilibrium moisture content of wood exposed in and outside (4 and 12%) were compared. Thermal modification of wood was performed at 190°C or 200°C for 2 h in industrial conditions. During the measurements, the moisture content of the modified and control samples was identical. The parameters compared included: modulus of elasticity, stress at proportionality limit, relative linear strain at proportionality limit and accumulated elastic energy. Changes in the mechanical parameters of wood induced by its thermal modification were found to depend on the modification temperature and wood moisture content.en-US
dc.formatapplication/pdf
dc.languageeng
dc.publisherUniversidad del Bio-Bioen-US
dc.relationhttps://revistas.ubiobio.cl/index.php/MCT/article/view/2555/2170
dc.rightsCopyright (c) 2016 Maderas. Ciencia y Tecnologíaen-US
dc.sourceMaderas-Cienc Tecnol; Vol. 18 No. 4 (2016); 577-586en-US
dc.sourceMaderas-Cienc Tecnol; Vol. 18 Núm. 4 (2016); 577-586es-ES
dc.source0718-221X
dc.source0717-3644
dc.subjectFraxinus excelsioren-US
dc.subjectmechanical propertiesen-US
dc.subjectThermowooden-US
dc.subjectwood densityen-US
dc.subjectwood modification.en-US
dc.titleMechanical parameters of thermally modified ash wood determined by compression in radial directionen-US
dc.typeinfo:eu-repo/semantics/article
dc.typeinfo:eu-repo/semantics/publishedVersion


This item appears in the following Collection(s)

Show simple item record