dc.descriptionThis study investigated the effect of the heat treatment on the wettability of the surface of juvenile teak (Tectona grandis) wood assessed by drop shape analyzer. Heartwood and sapwood samples were heat-treated at 180 and 200oC. Contact angle measurements were done every 5 s for 120 s using a KRÜSS DSA100. Heartwood had lower wettability than sapwood. Heat-treatment decreased the surface wettability of both heartwood and sapwood, especially in the wood treated at 200oC. Heartwood had lower wettability than sapwood, even after heat treatment.en-US
dc.formatapplication/pdf
dc.languageeng
dc.publisherUniversidad del Bio-Bioen-US
dc.relationhttps://revistas.ubiobio.cl/index.php/MCT/article/view/3050/3073
dc.sourceMaderas-Cienc Tecnol; Vol. 20 No. 2 (2018); 249-256en-US
dc.sourceMaderas-Cienc Tecnol; Vol. 20 Núm. 2 (2018); 249-256es-ES
dc.source0718-221X
dc.source0717-3644
dc.subjectChemical modificationen-US
dc.subjectcontact angleen-US
dc.subjectheartwooden-US
dc.subjecthygroscopicityen-US
dc.subjectsapwooden-US
dc.subjectTectona grandisen-US
dc.titleWettability of the surface of heat-treated juvenile teak wood assessed by drop shape analyzeren-US
dc.typeinfo:eu-repo/semantics/article
dc.typeinfo:eu-repo/semantics/publishedVersion


This item appears in the following Collection(s)

Show simple item record