Poly (l-lactide acid) improves complete nano-hydroxyapatite bone scaffolds through the microstructure rearrangement

Author
Shuai,Cijun

Nie,Yi

Gao,Chengde

Lu,Haibo

Hu,Huanlong

Wen,Xuejun

Peng,Shuping

Full text
https://scielo.conicyt.cl/scielo.php?script=sci_arttext&pid=S0717-34582012000600004
Abstract
Cracks often occur when nano-hydroxyapatite bone scaffolds are fabricated with selective laser sintering, which affect the performance of scaffolds. In this study, a small amount of poly (l-lactide acid) (PLLA) was added into nano-hydroxyapatite (nano-HAP) powder by mechanical blending in order to improve the sintering properties. The nano-HAP powder combined with 1wt % PLLA was sintered under different laser power (5W, 7.5W, 10W, 12.5W, 15W and 20W). The fabricated scaffolds were characterized using Scanning Electron Microscope (SEM), X-ray Diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR) and Micro Hardness Tester. The results showed that nano-HAP particles grew up quickly with the laser power increasing, and there were many strip-like cracks on the surface of sintering zone. The cracks gradually reduced until disappeared when the laser power increased to 15W, together with a great improvement of density. Large pores were observed on the specimen when the laser power further increases, accompanied with the decomposition of HAP into β-tricalcium phosphate (β-TCP) and tetracalcium phosphate (TTCP). And the optimum parameters were eventually obtained with laser power of 15W, scanning speed of 1000 mm/min, powder bed temperature of 150ºC, laser spot diameter of 2 mm and layer thickness of 0.2 mm. We summarized that the molten PLLA enhanced the particle rearrangement of nano-HAP by capillary force and may absorb thermal stress in laser sintering process, while PLLA would be oxidized gradually until completely excluded from the sintered nano-HAP scaffolds, which was confirmed by FTIR analysis. This study provides a novel method to improve the sintering properties of nano-HAP with no adverse effects which would be used in the application of bone tissue engineering potentially.
Metadata
Show full item record
Discipline
Artes, Arquitectura y UrbanismoCiencias Agrarias, Forestales y VeterinariasCiencias Exactas y NaturalesCiencias SocialesDerechoEconomía y AdministraciónFilosofía y HumanidadesIngenieríaMedicinaMultidisciplinarias
Institutions
Universidad de ChileUniversidad Católica de ChileUniversidad de Santiago de ChileUniversidad de ConcepciónUniversidad Austral de ChileUniversidad Católica de ValparaísoUniversidad del Bio BioUniversidad de ValparaísoUniversidad Católica del Nortemore

Browse

All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

My Account

LoginRegister
Dirección de Servicios de Información y Bibliotecas (SISIB) - Universidad de Chile
© 2019 Dspace - Modificado por SISIB